Ceramic for Dredger
DATE: November/2024
CUSTOMER ASSET: Flygt N3356 Pump
SEVERE ABRASION:
- Material loss on impeller blade edges
- Material loss on the wear ring
RECOMMENDED SOLUTION:
- Taurus TX5 — Fast-curing ceramic epoxy compound for abrasion – For filling severe wear. Packaging: 1 kg
- Taurus T58 — Ceramic epoxy metallic paste compound for abrasion – Restore surfaces. Packaging: 2 kg
- Taurus TS2 — Ceramic epoxy compound for corrosion and abrasion – Finish. Packaging: 1 kg
Industry: Municipal Public Drinking Water Company – Basic Sanitation
Operating Conditions: Ambient temperature Scope: Fill the metal to recover the lost surface, reconstruction of edges and corners of the impeller blades. Protection against severe wear. Protection against corrosion. Final finish of the protected surface.
INITIAL CONDITIONS


APPLICATION OF THE COATING ON THE WEAR RING



APPLICATION OF THE COATING ON THE IMPELLER



- Coating with 500 µm thickness
- Recovery offactory dimensions
- Smooth and glossy finish
- Equipment efficiency restored


Proper surface preparation is essentialfor the long-term performance of the coating. The exact requirements for preparation vary depending on the severity of the application, the expected service life, and the initial condition of the substrate.